A scratch or nick in aluminum alloy tubing can be repaired by burnishing provided the scratch or nick does not
A) exceed 10 percent of the tube diameter.
B) exceed 20 percent of the wall thickness of the tube.
C) appear in the heel of a bend in the tube.

 